I have two sets of parts. I found the heat spreader (copper) to be flat
(check yours against a straight edge). The aluminum is bowed inward
along the long axis. I used a succession of 220, 320 and 600 wet or dry
sandpaper on plate glass (used wet) smoothed the surface in about 90
minutes.

Perry W1COW